Ферритовые сердечники EE

| МОДЕЛЬ | Вес брутто |
Размер (мм) |
|||||
|
A |
Бмин |
C |
D |
E |
F |
||
|
ЭЛ27 |
33 |
27.0±0.6 |
19.0 мин. |
7.8±0.25 |
10.5±0.3 |
11.5±0.25 |
15.5±0.25 |
|
ЭЭ28 |
24 |
28.0±0.6 |
18.6 |
7.2±0.2 |
10.7±0.3 |
6.5±0.3 |
10.5±0.3 |
|
ЭЭ28.5 |
23 |
28.8±0.6 |
21.1 |
7.2±0.2 |
10.4±0.2 |
6.5±0.3 |
10.5±0.3 |
|
ЭЭ30/7 |
24 |
30.0±0.5 |
19.9±0.4 |
6.9±0.3 |
7.1±0.2 |
10.0±0.2 |
15.0±0.2 |
|
ЭЭ32/9,5 |
36 |
32.1±0.5 |
22.7 |
9.5±0.3 |
9.5±0.2 |
11.5±0.3 |
16.4±0.2 |
|
ЕЕ32/11 |
42 |
32.1±0.5 |
22.7 |
9.5±0.3 |
11.0±0.2 |
11.5±0.3 |
16.4±0.2 |
|
ЭЭ32.6/37/9,5 |
40 |
32.6±0.5 |
23.6 |
9.5±0.3 |
9.5±0.2 |
14.3±0.3 |
18.6±0.3 |
|
ЭЭ33А |
42 |
34.0±0.5 |
24 |
9.6±0.3 |
12.7±0.3 |
9.8±0.3 |
14.1±0.3 |
|
ЕЕ35/18 |
45 |
35.0±0.6 |
24.6 |
10.0±0.3 |
10.0±0.3 |
12.5±0.3 |
17.5±0.3 |
|
ЕЕ35/28 |
33 |
34.2±0.6 |
24 |
9.5±0.3 |
10.0±0.3 |
9.2±0.3 |
13.7±0.3 |
|
ЭЭ42%2ф15%2ф21 |
93 |
42.1±0.9 |
29.5 |
12.0±0.3 |
15.0±0.3 |
15.2±0.4 |
21.1±0.3 |
|
ЭЭ42/20/21 |
121 |
42.1±0.9 |
29.5 |
12.0±0.3 |
19.7±0.4 |
15.2±0.4 |
21.1±0.3 |
|
ЭЭ42/15/50 |
108 |
42.1±0.9 |
29.5 |
12.0±0.3 |
15.0±0.3 |
19.0±0.4 |
25.0±0.3 |
|
ЭЭ50 |
120 |
50.0±0.7 |
34.2 |
14.6±0.4 |
14.6±0.4 |
13.1±0.3 |
21.5±0.3 |
|
ЭЭ55А |
186 |
55.1±1.1 |
37.5 |
17.0±0.3 |
16.9±0.3 |
18.8±0.3 |
27.5±0.3 |
|
EE55B |
230 |
55.1±1.1 |
37.5 |
17.0±0.3 |
20.7±0.3 |
18.8±0.3 |
27.5±0.3 |
|
ЭЭ55С |
272 |
55.1±1.1 |
37.5 |
17.0±0.3 |
24.7±0.3 |
18.8±0.3 |
27.5±0.3 |
|
ЭЭ65А |
304 |
65.2±1.3 |
44.2 |
19.6±0.3 |
19.6±0.3 |
22.5±0.3 |
32.5±0.3 |
|
ЭЭ65Б |
416 |
65.2±1.3 |
44.2 |
19.6±0.3 |
27.0±0.3 |
22.5±0.3 |
32.5±0.3 |
|
ЭЭ70А |
412 |
70.5±1.5 |
48.0 |
16.7±0.5 |
24.5±0.6 |
24.6±0.6 |
35.5±0.5 |
|
ЭЭ70Б |
530 |
70.7±1.5 |
48.0 |
21.5±0.5 |
30.5±0.6 |
22.0±0.6 |
32.0±0.4 |
|
ЭЭ70/72 |
418 |
70.0±1.5 |
48.0 |
16.7±0.5 |
24.5±0.6 |
27.0±0.6 |
36.3±0.4 |
|
ЭЭ73/70 |
570 |
73.0±1.5 |
50.0 |
21.5±0.5 |
30.5±0.6 |
24.3±0.6 |
35.0±0.4 |
|
ЭЭ80/38/20 |
396 |
80.7±2.0 |
59.1 |
20.0±0.5 |
20.0±0.6 |
28.0±0.5 |
38.0±0.5 |
|
ЭЭ85А |
726 |
85.0±3.0 |
55.0 |
27.0±0.4 |
26.5±0.5 |
29.0±0.5 |
44.0±1.0 |
|
ЭЭ85Б |
860 |
85.0±3.0 |
55.0 |
27.0±0.4 |
31.5±0.5 |
29.0±0.5 |
44.0±1.0 |
|
ЕЕ100 |
1173 |
100.0+3.0/-1.5 |
72.0мин |
28.0±0.5 |
28.0±0.5 |
46.0±0.5 |
60.0±0.5 |
|
ЭЭ110 |
1700 |
110.0±3.0 |
74.2 |
36.0±1.0 |
36.0±1.0 |
38.7±0.6 |
57.0±0.5 |
|
ЭЭ130 |
2410 |
130.0±3.0 |
89.0 |
40.0±2.0 |
40.0±1.0 |
43.0±0.8 |
63.0±1.0 |
|
ЭЭ160 |
3400 |
160.0±3.0 |
120.0 |
40.0±2.0 |
20.0±1.5 |
64.0±1.0 |
83.0±1.0 |
|
ЭЭ188 |
6880 |
185.0±3.5 |
128.0 |
55.5±2.5 |
55.0±2.0 |
49.0±1.5 |
79.0±1.5 |
|
ЭЭ193 |
6880 |
193.0±3.5 |
132.0 |
58.0±2.0 |
59.0±2.0 |
49.0±1.5 |
79.0±1.5 |
|
ЭЭ210 |
5620 |
210.0±3.5 |
149.0 |
58.0±2.0 |
40.0±1.0 |
65.0±1.5 |
95.0±1.5 |
|
ЭЭ240 |
7000 |
240.0±4.0 |
176.0 |
56.0±3.0 |
40.0±1.5 |
86.5±1.0 |
117.0±1.0 |
|
МОДЕЛЬ |
Спецификация |
АЛ±25%(нХ/Н^2) |
ВЕС НЕТТО (г) |
||||||||
|
С1мм-1 |
Лемм |
Эмм2 |
Вемм3 |
ЗП40 |
Ж5К |
Ж7К |
Ж10К |
|
|||
|
CEEL27 |
0.867 |
70.0 |
80.7 |
5650.0 |
2500 |
|
|
|
27.0 |
||
|
ЭЭ28 |
0.620 |
51.7 |
82.9 |
4290.0 |
3500 |
|
|
|
21.6 |
||
|
ЭЭ28.5 |
0.660 |
51.4 |
77.6 |
4000.0 |
3300 |
|
|
|
21.0 |
||
|
ЭЭ30 |
1.089 |
65.4 |
60.0 |
3920.0 |
1980 |
|
|
|
19.4 |
||
|
ЭЭ32/9,5 |
0.890 |
74.6 |
86.3 |
6440.0 |
2500 |
|
|
|
32.0 |
||
|
ЕЕ32/11 |
0.746 |
74.6 |
100.0 |
7450.0 |
2900 |
|
|
|
37.5 |
||
|
ЭЭ32.6/37/9,5 |
1.026 |
85.5 |
83.0 |
7150.0 |
2200 |
|
|
|
36.0 |
||
|
ЭЭ33А |
0.589 |
67.4 |
114.0 |
7690.0 |
3700 |
|
|
|
39.0 |
||
|
ЕЕ35/18 |
0.810 |
80.7 |
100.0 |
8070.0 |
2700 |
|
|
|
41.0 |
||
|
ЕЕ35/28 |
0.753 |
67.7 |
89.9 |
6090.0 |
2900 |
|
|
|
30.0 |
||
|
ЭЭ42 |
0.534 |
97.0 |
182.0 |
17600.0 |
4700 |
|
|
|
86.0 |
||
|
ЭЭ42А |
0.415 |
97.4 |
235.0 |
22900.0 |
6100 |
|
|
|
115.0 |
||
|
ЭЭ42/15/50 |
0.630 |
113.0 |
179.0 |
20227.0 |
3400 |
|
|
|
100.0 |
||
|
ЭЭ50 |
0.425 |
95.8 |
226.0 |
21600.0 |
6100 |
|
|
|
115.0 |
||
|
ЭЭ55А |
0.432 |
123.0 |
285.0 |
35050.0 |
5000 |
|
|
|
168.0 |
||
|
ЭЭ55Б |
0.348 |
123.0 |
354.0 |
43700.0 |
6500 |
|
|
|
220.0 |
||
|
ЭЭ55С |
0.292 |
123.0 |
422.0 |
52130.0 |
7200 |
|
|
|
260.0 |
||
|
ЭЭ65А |
0.373 |
146.8 |
393.1 |
57728.4 |
5800 |
|
|
|
280.0 |
||
|
ЭЭ65Б |
0.274 |
147.0 |
535.0 |
78700.0 |
7800 |
|
|
|
380.0 |
||
|
ЭЭ70 |
0.344 |
159.0 |
409.0 |
73200.0 |
6500 |
|
|
|
380.0 |
||
|
ЭЭ70Б |
0.226 |
150.0 |
665.0 |
99800.0 |
9000 |
|
|
|
500.0 |
||
|
ЭЭ70/72 |
0.360 |
161.0 |
409.0 |
65800.0 |
10000 |
|
|
|
388.0 |
||
|
ЭЭ73/70 |
0.236 |
159.0 |
665.0 |
106000.0 |
9000 |
|
|
|
560.0 |
||
|
ЭЭ80/38/20 |
0.469 |
184.0 |
392.0 |
72300.0 |
6000 |
|
|
|
360.0 |
||
|
ЭЭ85А |
0.264 |
188.0 |
714.0 |
134000.0 |
8300 |
|
|
|
660.0 |
||
|
ЭЭ85Б |
0.220 |
189.0 |
859.0 |
162000.0 |
10000 |
|
|
|
750.0 |
||
|
ЕЕ100 |
0.344 |
270.000 |
784.000 |
222656.0 |
7300 |
|
|
|
1060.0 |
||
|
ЭЭ110 |
0.191 |
244.0 |
1280.0 |
312000.0 |
11000 |
|
|
|
1520.0 |
||
|
ЭЭ130 |
0.352 |
284.0 |
1600.0 |
454000.0 |
12000 |
|
|
|
2190.0 |
||
|
EE160 |
0.498 |
398.0 |
1600.0 |
637000.0 |
9000 |
|
|
|
2500.0 |
||
|
ЭЭ188 |
0.100 |
370.0 |
2940.0 |
1087800.0 |
21000 |
|
|
|
5700.0 |
||
|
ЭЭ193 |
0.100 |
380.0 |
3580.0 |
1360400.0 |
21000 |
|
|
|
5800.0 |
||
|
ЭЭ210 |
0.183 |
440.0 |
2400.0 |
1128000.0 |
13500 |
|
|
|
5400.0 |
||
|
ЭЭ240 |
0.235 |
556.4 |
2359.0 |
1312421.0 |
12500 |
|
|
|
5900.0 |
||